On this page
What is actually different
Both grades are austenitic stainless steels: iron with chromium, which forms the thin passive oxide film that makes steel "stainless", and nickel, which gives the austenitic structure, good weldability and formability. The difference is one alloying element and, in the L grades, a carbon limit.
| Grade (AISI / EN) | Chromium % | Nickel % | Molybdenum % | Carbon max % |
|---|---|---|---|---|
| 304 / 1.4301 | about 18-20 | about 8-10.5 | - | 0.07-0.08 |
| 304L / 1.4307 | about 18-20 | about 8-12 | - | 0.03 |
| 316 / 1.4401 | about 16-18 | about 10-14 | 2-3 | 0.07-0.08 |
| 316L / 1.4404 | about 16-18 | about 10-14 | 2-3 | 0.03 |
Typical ranges; exact limits differ slightly between ASTM and EN standards, so quote the standard in your specification.
What the molybdenum does
Molybdenum strengthens the passive film against localised attack by chlorides - pitting and crevice corrosion. A common way to compare grades is the pitting resistance equivalent number, PREN = %Cr + 3.3 × %Mo + 16 × %N. It comes out at roughly 18-20 for 304 and roughly 23-26 for 316L: a meaningful step, though not a licence to ignore chlorides altogether.
What the "L" does
When standard-carbon stainless is welded, the metal beside the weld spends time in a temperature range where carbon combines with chromium to form chromium carbides. The adjacent metal loses chromium and can corrode along grain boundaries - known as sensitisation or weld decay. Limiting carbon to 0.03% largely prevents it. For welded hoppers, tanks, pipework and funnels that touch product, specify 304L or 316L.
Where 304 fails and 316L survives
Uniform corrosion is rarely the problem with either grade. Failures on food and pharma machines are almost always pitting (small, deep holes) or crevice corrosion (under gaskets, clamps and deposits), and the usual driver is chloride. Common sources on packaging machines:
- Product: salted snacks, brine, pickles, sauces, soy, ketchup and other salty or acidic products; some syrup and oral-liquid formulations.
- Cleaning: chlorine-based sanitisers such as sodium hypochlorite, especially when used strong, hot or left to dry on the surface.
- Water: washdown water with high chloride content, and evaporation that concentrates it on horizontal surfaces.
- Environment: coastal plants and export destinations with salty air.
A commonly quoted rough guide for water at ambient temperature puts the practical chloride limit for 304 at around 200 mg/l and for 316 at around 1,000 mg/l. Temperature, crevices and stagnant deposits all lower these limits, so use them to spot risk, not to design to the edge.
Hypochlorite left overnight on a 316L hopper will still pit it. Follow the chemical supplier's concentration and contact time, rinse with clean water and let surfaces drain and dry.
Design matters as much as grade. Horizontal ledges, lap joints and crevices under clamps hold water and residue, and that is where pitting starts. The same washdown zone also needs electrical components rated for it - see IP65 vs IP66 vs IP69K - because a corroded sensor housing or a flooded junction box stops the line just as surely as a pitted hopper.
Where each grade belongs on a machine
Specifying 316L everywhere is expensive and unnecessary; specifying 304 everywhere is a false saving for product contact. Common practice on packaging machines:
| Part | Typical specification | Why |
|---|---|---|
| Pharma product contact (hoppers, filling nozzles, pistons, pipework, auger and funnel) | 316L, polished | Expected by most pharma URSs; verified at IQ |
| Food contact, salty, acidic or wet product | 316L | Chloride and acid resistance |
| Food contact, dry non-salty product (grains, sugar, dry powders) | 304 is often adequate | Low corrosion load; decide with the cleaning method |
| Frames, guards, covers in washdown areas | 304 | Splash and cleaning exposure without product contact |
| Base frames in dry halls (cartoners, case packers, palletisers) | 304, or painted mild steel where hygiene rules allow | Cost; no product contact |
| Fasteners | A2 (304) generally, A4 (316) in contact or wet zones | Match the surrounding material to avoid weak points |
| Change parts | 316L, or food-grade engineering plastics | Contact with containers; weight for quick change |
For a multihead weigher packing salted namkeen or a liquid filling machine handling syrups, product-contact parts in 316L are the sensible default. For a cartoner, where the product is already sealed in a bottle or blister, 304 guards over a 304 or painted frame are normal.
Surface finish: specify Ra, not grit
Smooth surfaces clean faster and give bacteria and residue fewer places to hide. Surface roughness is specified as Ra in micrometres and measured with a portable profilometer. Common practice:
- Food product contact: Ra 0.8 µm or better is widely specified in hygienic-design guidance.
- Pharma product contact: often Ra 0.5 µm or better, and 0.4 µm or electropolished for liquid-contact parts, as set in the URS.
- Non-contact surfaces: mill finish (2B) or brushed; the concern is appearance and easy wiping.
Grit numbers ("240-grit polish") are not a specification: the resulting Ra depends on the starting surface, the abrasive and the operator. Write the Ra value into the URS and ask for measured readings on the critical parts. Welds on contact surfaces should be ground flush and polished to the same finish.
Material certificates: what EN 10204 3.1 means
EN 10204 defines types of inspection documents for metallic products. The one that matters for product-contact steel is type 3.1:
| Type | What it is | Enough for contact parts? |
|---|---|---|
| 2.1 | Declaration of compliance with the order, no test results | No |
| 2.2 | Test report with non-specific results (typical values for the product) | No |
| 3.1 | Inspection certificate with results of tests on the actual heat or batch, validated by the manufacturer's authorised inspection representative, independent of production | Yes - the usual requirement |
| 3.2 | As 3.1, also validated by the purchaser's representative or a third party | Where the URS demands it |
A certificate is only useful if it is traceable to the part. The heat number on the 3.1 certificate should appear in a material traceability list that says which components were cut from which sheet or bar. Materials of construction are verified during installation qualification, and a certificate that cannot be tied to a part is a common IQ gap.
Welding and passivation
Good steel can be spoiled in the workshop. What to look for:
- TIG welding with matching filler (308L for 304, 316L for 316L) and argon back-purging on tubes and closed sections, so the inside of the weld is not oxidised.
- Heat tint removed by pickling or mechanical finishing. Discoloured weld zones have reduced corrosion resistance.
- Passivation of product-contact parts with nitric or citric acid after fabrication, to rebuild a clean, uniform passive film.
- No carbon-steel contamination. Dedicated grinding discs, wire brushes and clamps for stainless. Iron particles from shared tools rust within days and look like the stainless is failing.
How to check what you are buying
Most grade disputes are settled with a handheld PMI (positive material identification) analyser. X-ray fluorescence (XRF) reads chromium, nickel and molybdenum in seconds, so it clearly separates 304 from 316. It cannot measure carbon, so it cannot distinguish 316 from 316L; that needs optical emission spectroscopy (OES) or the traceable 3.1 certificate. A magnet is not a test: austenitic grades can become slightly magnetic after cold working, and some low-nickel grades are barely magnetic at all.
316L on the visible hopper but 304 on the hidden funnel or pipework; 200-series (low-nickel, high-manganese) steel sold as "SS" for frames and guards; thinner sheet than quoted; certificates for a different heat than the parts; welds ground but not passivated. A 10-minute PMI check at FAT catches most of them.
Cost factors
316L costs more than 304 per kilogram because of its higher nickel and added molybdenum; indicative market prices in 2026 typically put it around 30-50% higher, moving with nickel prices. On a finished machine the difference is smaller than that suggests, because product-contact parts are a small share of total steel weight. Machining, polishing and documentation often cost more than the steel itself. At MEF we quote the grade of each assembly in the proposal, so there is no ambiguity about what "SS construction" means.
Frequently asked questions
Is SS304 food grade?
Why do pharma machines use SS316L for contact parts?
Can an XRF gun tell 316 from 316L?
What surface finish is needed for food contact parts?
Is 202 stainless steel acceptable for packaging machines?
References
- BSSA: Comparison of 304 or 316 and 304L or 316L compositions and effect on corrosion resistance
- IMOA: Molybdenum-grade stainless steels FAQ
- Nickel Institute: Design guidelines for the selection and use of stainless steels
- worldstainless: Categories and grades of stainless steel
- EU GMP Annex 15: Qualification and Validation
Regulatory text changes. Always check the current version of a regulation before relying on it; this article reflects our reading as of 29 Sep 2026 and is not legal advice.